Anodizing successfully combines science with nature to create one of the world's best metal finishes.
It is an electrochemical process that thickens
and toughens the naturally occurring protective oxide. The resulting
finish, depending on the process, is the second hardest substance known
to man, second only to the
diamond. The anodic coating is part of the metal, but has a porous
structure which allows secondary infusions, (i.e. organic and inorganic
coloring, lubricity aids, etc.)
Anodizing Definitions and Methods
While the chemical anodizing process remains the same
for all applications, the mechanical methods vary according to the two
physical types and shapes of metals used:
|
Appearance options and quality are improved
through the use of dyes and special pretreatment procedures. This makes
the aluminum look like pewter, stainless steel, copper, brushed bronze
or polished brass and can also be
colored with brilliant blues, greens, reds, and many varieties of
metallic gold and silver.
The unique dielectric properties of an anodized finish offer many opportunities for electrical applications.
The surface of the aluminum itself is toughened
and hardened to a degree unmatched by any other process or material. The
coating is 30 percent thicker than the metal it replaces, since the
volume of oxide produced is
greater than that of the metal replaced.
The resulting anodic coating is porous, allowing relatively easy coloring and sealing.
Hard Anodizing is a
term used to describe the production of anodic coatings with film
hardness or abrasion as their primary characteristic. They are usually
thick by normal anodizing standards
(greater than 25 microns) and they are produced using special
anodizing conditions (very low temperature, high current density,
special electrolytes). They find application in the engineering industry
for components which
require a very wear resistant surface such as piston,
cylinders and hydraulic gear. They are often left unsealed, but may be
impregnated with materials such as waxes or silicone fluids to give
particular surface properties.
Batch and Coil Anodizing
Batch and coil anodizing are accomplished in five carefully controlled, calibrated, quality-tested stages:
1. Cleaning. Alkaline and/or acid cleaners remove grease, and surface dirt.
2. Pre-Treatment
- Etching. An appealing matte surface finish is created with hot solutions of sodium hydroxide to remove minor surface imperfections. A thin layer of aluminum is removed to create a matte or dull finish.
- Brightening. A near mirror finish is created with a concentrated mixture of phosphoric and nitric acids which chemically smooths the aluminum's surface.
3. Anodizing. The anodic film
is built and combined with the metal by passing an electrical current
through an acid electrolyte bath in which the aluminum is immersed. The
coating thickness and surface
characteristics are tightly controlled to meet end product
specifications.
4. Coloring. Coloring is achieved in one of four ways:
- Electrolytic Coloring (The two-step method) - After anodizing, the metal is immersed in a bath
- Integral Coloring - This so-called one-step process combines anodizing and coloring to simultaneously form and color the oxide cell wall in bronze and black shades while more abrasive resistant than conventional anodizing. It is the most expensive process since it requires significantly more electrical power.
- Organic Dyeing - The organic dyeing process produces a wide variety of colors. These dyes offer vibrant colors with intensities that cannot be matched by any other paint system in the market. They can also provide excellent weather-fastness and light-fastness. Many structures built with these finishes have lasted more than 20 years. The color range can be broadened by over-dyeing the electrolytic colors with the organic dyes for a wider variety of colors and shades. This method is relatively inexpensive and involves the least amount of initial capital of any other coloring process.
- Interference Coloring - An additional coloring procedure, recently in production, involves modification of the pore structure produced in sulfuric acid. Pore enlargement occurs at the base of the pore. Metal deposition at this location produces light-fast colors ranging from blue, green and yellow to red. The colors are caused by optical-interference effects, rather than by light scattering as with the basic electrolytic coloring process. Further development will produce a greater variety of colors.
Here is detailed information comparing two of the most common coloring processes used: (note - these two types of processes will not produce identical colors; both can be overdyed. Source: Aluminum Anodizers Council Technical Bulletin #1-94, issued January, 1994.) See below.
5. Sealing. This process closes
the pores in the anodic film, giving a surface resistant to staining,
abrasion, crazing and color degradation.
Quality control. Throughout the entire anodizing
process, AAC members monitor the process and quality of the product. The
application of electrical power and color is preprogrammed and verified
on all batches and coils.
This quality control ensures uniformity to end
product specifications for film thickness, density, abrasion resistance,
corrosion resistance, color uniformity, fade resistance, reflectivity,
image clarity, insulative properties,
adhesion and sealing.
In many cases, AAC members use Statistical Process Control (SPC) methods to meet rigorous quality assurance standards.
Comparison of A32/A42 and A34/A44 Colored Aluminum Anodic Finishes
A32 & A42 | A34 & A44 | |
---|---|---|
Generic Names
|
Integral One Step Architectural Hardcoat |
Electrolytic Coloring Two Step |
Representative Trade Names
|
Duranodic Kalcolor Permanodic |
Anolok Sandocolor Colormax |
Colors
|
Champagnes, Bronzes, Blacks, Grays | Champagnes, Bronzes, Blacks, Pinks, Burgundies |
Exterior Durability
|
Excellent | Excellent |
Color Match
|
Good | Excellent |
Color Reproducibility
|
Good | Excellent |
Alloy Sensitivity
|
High | Low |
Cost to Produce
|
Moderate | Low |
Energy Required to Produce
|
High | Low |
Availability-Batch Processing
|
Limited | Low |
Availability-Coil Processing
|
Unavailable | Low |